Conversion coatings (phosphate layer) of aluminium

From Efficiency Finder
Revision as of 14:04, 18 November 2010 by Breka (Talk | contribs) (New page: Back to EFFICIENCY FINDER FOR METAL INDUSTRY *;Typical parameters of the process {| border="1" | align="center" style="background:#2266CC;"|'''Process''' | al...)

(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to: navigation, search

Back to EFFICIENCY FINDER FOR METAL INDUSTRY


  • Typical parameters of the process
Process Temperature [°C] Heat transfer medium Residence time Chemicals Concentration Details Literature
Alkali phosphoting of aluminium 40-70 (can be lowered to 25-35°C with special bath comeditions) 5-10 sec Aluminium, phosphate and fluoride solutions 2-15 g/l spaying of strip material BAT for the surface treatment of metals & plastics, 2006
1-3 min spaying or dipping of individual parts