Difference between revisions of "Laquering of steel cast products"
From Efficiency Finder
(Created page with "Back to Subsection DC metals ''' Laquering in the automotive industry ''' {| border="1" | align="center" style="background:#2266CC;"|'''Process''' | align="center" style...") |
|||
(2 intermediate revisions by the same user not shown) | |||
Line 1: | Line 1: | ||
− | Back to [[Subsection | + | Back to [[Subsection DJ metals|EFFICIENCY FINDER FOR METAL INDUSTRY]] |
− | ''' | + | ''' Typical parameters for the automotive industry ''' |
{| border="1" | {| border="1" | ||
Line 20: | Line 20: | ||
|} | |} | ||
− | + | Back to [[Subsection DJ metals|EFFICIENCY FINDER FOR METAL INDUSTRY]] | |
− | Back to [[Subsection | + |
Latest revision as of 08:49, 6 September 2016
Back to EFFICIENCY FINDER FOR METAL INDUSTRY
Typical parameters for the automotive industry
Process | Temperature [°C] | Heat transfer medium | Residence time | Details | Literature |
Drying after rinsing | <60°C | air | continious | Hans-Hermann Braess, U. S. (2012). Vieweg Handbuch Kraftfahrzeugtechnik. Vieweg+Teubner Verlag | |
Drying after laquering (after base coat, clear lacquer) | 170 – 220°C | air | continious | ||
Spray booth | 22 – 26°C | air | continious | ||
Thermal post-combustion | 750 °C | exhaust gas | continious |