Back to Subsection DC metals
Typical paramters for the automotive industry
Process | Temperature [°C] | Heat transfer medium | Residence time | Details | Literature |
Drying after rinsing | <60°C | air | continious | Hans-Hermann Braess, U. S. (2012). Vieweg Handbuch Kraftfahrzeugtechnik. Vieweg+Teubner Verlag | |
Drying after laquering (after base coat, clear lacquer) | 170 – 220°C | air | continious | ||
Spray booth | 22 – 26°C | air | continious | ||
Thermal post-combustion | 750 °C | exhaust gas | continious |