Laquering in the automotive industry

Process Temperature [°C] Heat transfer medium Residence time Details Literature
Drying after rinsing <60°C air continious Hans-Hermann Braess, U. S. (2012). Vieweg Handbuch Kraftfahrzeugtechnik. Vieweg+Teubner Verlag
Drying after laquering (after base coat, clear lacquer) 170 – 220°C air continious
Spray booth 22 – 26°C air continious
Thermal post-combustion 750 °C exhaust gas continious