Difference between revisions of "Solvent degreasing of steel coil"

From Efficiency Finder
Jump to: navigation, search
m (Protected "Solvent degreasing of steel coil" [edit=autoconfirmed:move=autoconfirmed])
 
(3 intermediate revisions by 2 users not shown)
Line 1: Line 1:
Back to [[Subsection DJ metals|EFFICIENCY FINDER OF METAL INDUSTRY]]
+
Back to [[Subsection DJ metals|EFFICIENCY FINDER FOR METAL INDUSTRY]]
  
  
Line 17: Line 17:
  
  
Back to [[Subsection DJ metals|EFFICIENCY FINDER OF METAL INDUSTRY]]
+
Back to [[Subsection DJ metals|EFFICIENCY FINDER FOR METAL INDUSTRY]]

Latest revision as of 08:46, 6 September 2016

Back to EFFICIENCY FINDER FOR METAL INDUSTRY


  • Typical parameters of the process
Process Temperature [°C] Degreasing agent Concentration Details Literature
Degreasing in coating processes 60-85 Alcaline containing phosphate, containing mainly sodium hydroxides, orthophosphates and surfactant compounds 40-50 g/l pH~13 BAT for the surface treatment of metals & plastics, 2006


Back to EFFICIENCY FINDER FOR METAL INDUSTRY